A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Good silicon etching woth RIE
Good silicon etching woth RIE
2011-11-22
Judith Linacero Blanco
Good silicon etching woth RIE
Judith Linacero Blanco
2011-11-22
Hello,

I'm trying to record 1 micron depth with 1.4 micron silicon mask AZ1512.
With depth but I have a huge roughness on the wall! I use a 80 Plasmalab RIE
with HBr 50sccm sparámetros, 20MT and 250W. Can anyone help?