MEMSnet Home: MEMS-Talk: Optical absorbing material
Optical absorbing material
2012-01-05
Mike Whitson
2012-01-06
Glenn Silveira
2012-01-07
Alasdair Rankin
2012-01-05
Dean Hopkins
2012-01-06
Mike Whitson
2012-01-07
Shay
2012-01-06
Marc Reinig
2012-01-07
Dean Hopkins
Optical absorbing material
Mike Whitson
2012-01-05
Hello all,

I'm trying to identify possible materials / vendors for a broadband (vis-MWIR)
optical absorbing layer to be integrated in an optical MEMS device.  In the
past, we've used a spin-coatable black polyimide for the purpose (purchased from
Brewer), but they no longer make or sell the material.  Wondering if anyone has
suggestions for an alternative vendor or material.  What we're looking for:

* High broadband optical absorption.  Ideally a single material spanning the
entire range from ~300-5000 nm would be good, but sets of materials with broad
absorption bands (eg one for visible, one for 3000 - 5000 nm) would also work.
Ideally absorption should be high enough to perform well at sub-wavelength
coating thicknesses.

(Good absorption at i- and g-line wavelengths to act as a kind of BARC during
photolithography would be a bonus, but not a requirement.)

* Spin coatable.

* Electrical resistivity as high as possible.  Given that one way to make such a
material is by impregnating carbon black in a polymer matrix, I understand that
getting a truly insulating material may be tough.

* Patternable.  Ideally a diretly photopatternable material would be wonderful;
if not, something amenable to a lift-off or etch process (say O2 RIE with a hard
mask) would be sufficient.

* Long life.  This will be a permanent part of the optical device; polymers that
can be crosslinked or otherwise cured would be preferable.

If anyone has suggestions for vendors or even particular materials, I'd be
grateful.

-Mike

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing