MEMSnet Home: MEMS-Talk: Etching recipe of AlPO film
Etching recipe of AlPO film
2012-01-09
zhanggeng
Etching recipe of AlPO film
zhanggeng
2012-01-09
Hi everyone,

Can anybody share a etching recipe of AlPO (  Al2O3-3x(PO4)2x   ) film? I have
deposited the AlPO film(150nm) by a solution-process but no experience in
etching it. Any advice will be much appreciated.

Thanks
GengZhang