MEMSnet Home: MEMS-Talk: Si/SiO2/Au ohmic contact problem with and without adhesion promoter layer
Si/SiO2/Au ohmic contact problem with and without adhesion promoter layer
2012-03-07
Mohd.Yusuf
Si/SiO2/Au ohmic contact problem with and without adhesion promoter layer
Mohd.Yusuf
2012-03-07
Dear All,

i need to have ohmic contact (good electrical contact) between:
silicon/sio2 (siO2 thickness 300nm) and Au.   in short i need to have gold
electrodes of Gold on si/sio2 substrate.

i used 5nm Ni as adhesion promotion layer below 100nm Au but it is not
helping. i cannot use Ti or Cr for some reasons. Also, i cannot use any
other metal except Gold.

all evaporation are done using e-beam evaporator or normal thermal
evaporator. patterns are in few 10s of microns to 200microns parallel
lines. i used photolithographic (lift-off) process and also shadowmasking
process both. but in both process i am not able to have good ohmic contact
of Au deposited on SiO2.   i also did O2 plasma cleaning before metal
deposition, doesn't help.

do you know whether i need any annealing or RTA (duration, temp) after
metal depositions ? or do i need to do any surface treatment before
metalization. the only adhesion promotion layers which i can use is Ge or
Ni.

i did and am doing a lot of literature search on Si-SiO2/Ni/Au metalization
but i am not able to get proper paper as we have very few subscribed
journals. everybody says that use Cr or Ti or NiAu alloy as adhesion
promotion layer but not more details are given.

thanks a lot in advance for ur help ...guidance.

regards
ysm

**
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing