MEMSnet Home: MEMS-Talk: RIE Etching Cr with PMMA Mask
RIE Etching Cr with PMMA Mask
2012-04-25
Judith Linacero
2013-01-12
冯跃
RIE Etching Cr with PMMA Mask
冯跃
2013-01-12
The O2(90sccm)+CF4(6sccm) at relatively high pressure could remove 50
nm-thick Cr within 3 min.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group