Chemical Mechanical Polishing
2013-03-12
Xiaoguang Liu
2013-03-13
Ioannis Nikolaou
2013-03-13
Darius Virzonis
Chemical Mechanical Polishing
Xiaoguang Liu
2013-03-12
Dear MEMS community

Our lab has been thinking about acquiring a chemical mechanical polishing
tool. We are tight in budget so I'm wondering what would be an economical
solution. Would it be possible for us to build one ourselves? What caveats
do we need to look for if we are looking for a second-hand one? We are
interested in planarizing photoresist (with plated metal) and silicon
primarily. We typically process small pieces of samples (1in^2 or so) and
seldom do full wafers.

Many thanks.

Leo

--
Xiaoguang "Leo" Liu
Assistant Professor
Electrical and Computer Engineering, Davis MM-Wave Research Center
University of California, Davis
3169 Kemper Hall, One Shields Avenue, Davis, CA, 95616
[email protected]
http://ucdart.net
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing