MEMSnet Home: MEMS-Talk: Resist thickness for nitride etch
Resist thickness for nitride etch
2013-05-08
Haider, Ahmad M
2013-05-08
Lou Chomas
2013-05-09
Haider, Ahmad M
2013-05-09
Andrew Sarangan
2013-05-09
Andrew Sarangan
2013-05-09
MRC gmail
2013-05-09
Haider, Ahmad M
2013-05-09
Robert Ditizio
Resist thickness for nitride etch
Haider, Ahmad M
2013-05-09
Hi Lou,

What do you mean by "Be careful to account for any etching into the substrate if
you are using a profilometer to measure the thickness." I use the dektak
profilometer to measure the thickness in order to verify if the RIE plasma
etcher was able to remove all exposed silicon nitride.

Thanks,
Ahmad

----- Original Message -----
From: "Lou Chomas" 
To: "General MEMS discussion" 
Sent: Wednesday, May 8, 2013 5:09:30 PM
Subject: Re: [mems-talk] Resist thickness for nitride etch

Ahmad,    That depends a lot on your process.  I would recommend putting some
resist down with your pattern on a test wafer and etching for some amount of
time.  Pick something less than your total etch, but not too short.  Measure the
thickness of the resist before and after and then you can calculate whether the
thickness will be sufficient.  Be careful to account for any etching into the
substrate if you are using a profilometer to measure the thickness.  If your
recipe has a lot of oxygen, the rate against the resist will likely be very
high.
-Lou
> Date: Wed, 8 May 2013 16:29:49 -0400
> From: [email protected]
> To: [email protected]
> Subject: [mems-talk] Resist thickness for nitride etch
>
> Hi
>
> I am trying to do an anisotropic etch of 400 nm nitride layer in a RIE
machine. A portion of the nitride is protected by a resist layer on top of it.
Can you tell approximate how much thickness of resist would I need so that the
resist doesn't get stripped off during the nitride etch?
>
> Thanks,
> Ahmad
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

--
Ahmad Haider
PhD Student, School of Mechanical Engineering
Georgia Institute of Technology, Atlanta
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review