<110>-oriented Si wafers
2013-08-08
Justin Hannigan
<110>-oriented Si wafers
Justin Hannigan
2013-08-08
We're interested in some silicon wafers with orientation <110>.  (150mm
or 200mm diameter would be fine.)  Can anyone recommend a good source?

--
Justin M. Hannigan, Ph.D.
Process Development Engineer
LightSmyth Technologies,Inc.
875 Wilson St, Unit C
Eugene, OR 97402
Tel: 541-431-0026
www.lightsmyth.com


!DSPAM:5202f976241931304452542!


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
Nano-Master, Inc.