KMPR is another option you can check into.

http://microchem.com/Prod-KMPR.htm


On Mon, Sep 23, 2013 at 2:02 AM, Ricky Anthony wrote:

> Hi,
>
> I was wondering if anyone can suggest me thick permanent photoresist
> (70-100um) single spin. I know of SU-8 but I need resists which have lower
> CTE~ (as low as 20ppm/C) or close.
>
> Many Thanks,
>
> Ricky Anthony
> Tyndall National Institute
> Ireland
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering
The Branford Group