MEMSnet Home: MEMS-Talk: TMAH reaction with copper
TMAH reaction with copper
2013-09-30
Ricky Anthony
2013-09-30
Yuksek, Nuh S. (MU-Student)
2013-10-01
André Bödecker
2013-10-03
Ricky Anthony
2013-10-16
André Bödecker
TMAH reaction with copper
Ricky Anthony
2013-09-30
Hi All,

I am working with Metal Ion free developers (MIF). I find that some TMAH based
MIF developers react with copper to form complex, while others do not even
though they are TMAH MIF based. What could be the possible explanation behind
this?

Many Thanks,

Ricky Anthony

Microsystems Center
Tyndall National Institute
University College Cork
Cork, IRELAND

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing