MEMSnet Home: MEMS-Talk: Mask patterns for lithography resolution
Mask patterns for lithography resolution
2013-10-15
SHANE GUO
2013-10-15
Michel van de Moosdijk
2013-10-16
Bill Moffat
Mask patterns for lithography resolution
Bill Moffat
2013-10-16
If it still exists I would start with Bay Area Chrome Users Society. A loose
knit society of bay area mask makers.  Bill Moffat

-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of Michel van
de Moosdijk
Sent: Tuesday, October 15, 2013 9:34 AM
To: General MEMS discussion
Cc: [email protected]
Subject: Re: [mems-talk] Mask patterns for lithography resolution

Benchmark Technologies has a lot of experience in masks for testing litho

Verstuurd vanaf mijn iPad

> Op 15 okt. 2013 om 18:30 heeft "SHANE GUO"  het
volgende geschreven:
>
> Hi all,
> I am working with SU-8 molds for making microfluidic devices through
softlithography process. I am supposed to test our fabrication capability,
lithography resolution and spin coating uniformity. I need to design a mask
including features that can help me to find out the above things.
> Do you guys know where I can find such mask patterns or references for
designing such patterns?
> Thank you in advance for your help.
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>

--
The information contained in this communication and any attachments is
confidential and may be privileged, and is for the sole use of the intended
recipient(s). Any unauthorized review, use, disclosure or distribution is
prohibited.  Unless explicitly stated otherwise in the body of this
communication or the attachment thereto (if any), the information is provided on
an AS-IS basis without any express or implied warranties or liabilities.  To the
extent you are relying on this information, you are doing so at your own risk.
If you are not the intended recipient, please notify the sender immediately by
replying to this message and destroy all copies of this message and any
attachments. ASML is neither liable for the proper and complete transmission of
the information contained in this communication, nor for any delay in its
receipt.

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review