MEMSnet Home: MEMS-Talk: natural oxidation of copper thin film
natural oxidation of copper thin film
2014-03-05
κΉ€λ•μˆ˜
2014-03-05
Ricky Anthony
natural oxidation of copper thin film
Ricky Anthony
2014-03-05
Hi,

Copper does not oxidize in such a short time. But I would suggest that after
resist patterning do a 2 mins (H2SO4 :DI in 1:10)+N2 dry and then electroplate
Nickel.


Ricky

-----Original Message-----
From: [email protected] [mailto:mems-talk-
[email protected]] On Behalf Of ???
Sent: 05 March 2014 09:06
To: General MEMS discussion
Subject: [mems-talk] natural oxidation of copper thin film

Hi.

at first, I want you to understand that I don't know english very well.


I performed Cu deposition process(3000β„«) for forming electrode(for
electroplating)

and I wil perform PR patterning on Cu layer and Ni electroplating.

I would like to know if Cu film can oxidize naturally after 1~2 days.

if Cu film oxidizes, it affects Ni electroplating??

ex) oxidized Cu layer can I no longer use for electrode for electroplating???


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
The Branford Group