Leily Majidi
2016-02-22
André Bödecker
Silicone-plastic bonding
Leily Majidi
2016-02-18
Hello all,

I am having problem bonding silicone chip which is coated with chromium to
Lexan ploycarbonat cover. The bonding seems good, however I have leakage in
my device at the edges.
I have microchannels on my chip and I need to have a flow through
microchannels. I used SU8-2 with the thickness around 5 um. After spin
coating, I baked two parts and then used UV and finally post bake.

I appreciate it if you share your knowledge with me.
Thanks!
Leily
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Tanner EDA by Mentor Graphics