Better resolution for desktop publishing masks
1999-02-04
John R Lodmell
Better resolution for desktop publishing masks
John R Lodmell
1999-02-04
        I have recently used a commercial printer to make a mask on printer's
film.  He used a Linotronic printer with 2540 dpi.  The mask gave us about 25
micron resolution, which I understand is pretty typical.
        I would really like about 10 micron resolution, but our
photolithography system does not have reduction capability (only 1:1).  Does
anyone know how to get closer to 10 microns?  Try to find higher dpi
capabilities?  Commercially available reduction to make a new mask from the
existing mask?
        Any suggestions would be appreciated.

John Lodmell
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review