A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Sealing Materials for Packaging
Re: Sealing Materials for Packaging
1999-08-17
Sandra Bishop
Re: Sealing Materials for Packaging
Sandra Bishop
1999-08-17
This is a multi-part message in MIME format.

------=_NextPart_000_0007_01BEE8BC.B6F8B1C0
Content-Type: multipart/alternative;
        boundary="----=_NextPart_001_0008_01BEE8BC.B6F8B1C0"


------=_NextPart_001_0008_01BEE8BC.B6F8B1C0
Content-Type: text/plain;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable

The black glass like material you are refering to is Apiezon Wax W, =
which is sometimes referred to as "black wax".

This would be melted up to 140=B0C where it will become a pourable =
liquid and can be used to fix and seal devices on cooling and is an =
electrical insulator.

We are the manufacturer of this product and would be pleased to discuss =
the product application or send more information, please contact us at =
tel +44 161 875 4443, fax +44 161 875 2695, e-mail [email protected]


Sandra Bishop
Marketing Manager
Apiezon Products, M&I Materials Ltd
If you have received this e-mail in error, please immediately notify =
Sandra Bishop by telephone at +44(0) 161 875 4443 or email to =
[email protected].
=20


________________________________________________________________________________
This message has been checked for all known viruses by the Star Screening System
http://academy.star.co.uk/public/virustats.htm
------=_NextPart_001_0008_01BEE8BC.B6F8B1C0
Content-Type: text/html;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable









The black glass like material you = are refering=20 to is Apiezon Wax W, which is sometimes referred to as "black=20 wax".
 
This would be melted up to 140°C = where it=20 will become a pourable liquid and can be used to fix and seal devices on = cooling=20 and is an electrical insulator.
 
We are the manufacturer of this = product and=20 would be pleased to discuss the product application or send more = information,=20 please contact us at tel +44 161 875 4443, fax +44 161 875 2695, e-mail = [email protected]
 
 
Sandra Bishop
Marketing = Manager
Apiezon=20 Products, M&I Materials Ltd
If you have received this e-mail in = error,=20 please immediately notify Sandra Bishop by telephone at +44(0) 161 875 = 4443 or=20 email to [email protected]= .
 

________________________________________________________________________________
This message has been checked for all known viruses by the Star Screening System
http://academy.star.co.uk/public/virustats.htm
------=_NextPart_001_0008_01BEE8BC.B6F8B1C0-- ------=_NextPart_000_0007_01BEE8BC.B6F8B1C0 Content-Type: text/x-vcard; name="Sandra Bishop.vcf" Content-Transfer-Encoding: quoted-printable Content-Disposition: attachment; filename="Sandra Bishop.vcf" BEGIN:VCARD VERSION:2.1 N:Bishop;Sandra FN:Sandra Bishop ORG:Apiezon Products, M&I Materials Ltd TITLE:Marketing Manager TEL;WORK;VOICE:+44 (0)161 875 4443 TEL;WORK;FAX:+44 (0)161 875 2695 ADR;WORK:;;PO Box 136;Manchester;;M60 1AN;UK LABEL;WORK;ENCODING=3DQUOTED-PRINTABLE:PO Box 136=3D0D=3D0AManchester = M60 1AN=3D0D=3D0AUK URL: URL:http://www.apiezon.com EMAIL;PREF;INTERNET:[email protected] REV:19990817T132803Z END:VCARD ------=_NextPart_000_0007_01BEE8BC.B6F8B1C0--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.
Tanner EDA by Mentor Graphics