Hi Alex,
for LIGA prototyping try this:
http://www.ntb.ch/Infos/IMS/Projekte/LC-LIGA.html

At this institute a low cost LIGA process is being develoved. Maybe it would be
interesting for your prototyping, maybe they can help you otherwise. The webpage
is in german, but they speak english too.

Cheers,
Ralf G. Longwitz.

Research Assistant
Microsystems integration group
Swiss Fed. Inst. of Technology
_______________________________

EPFL-DMT-IMS  BM 3.125
http://dmtwww.epfl.ch/~rlongwit
Tel: +41.21-693 6727
Fax: +41.21-693 5950
_______________________________


> Dear researchers,
>
> I have just heard that MCNC/Cronos is no longer ofering LIGA
> multiproject run.  Does anyone know an alternative for small scale
> prototyping LIGA work?  Thanking you,
>
> alex
>
> --
> Alex Freeman, Ph.D
> Research Scientist
> Zyvex
> 1321 N. Plano Rd, #200
> Richardson, TX 75081
> 972-235-7881 x219
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review