MEMSnet Home: MEMS-Talk: Need SiO2 Etch Modeling Program
Need SiO2 Etch Modeling Program
1995-11-22
Justin Mansell
Need SiO2 Etch Modeling Program
Justin Mansell
1995-11-22
I need to be able to predict the effects of an isotropic or partly anisotropic
(HF or PACE) etch of SiO2 with on a simple surface (a staircase of levels). Can
anyone recommend a way of doing this?

Thanks,
Justin.
Justin Mansell        | "The voyage will be a success only
1626 E. 115th St. #102| if the ships do not collide AND each
Cleveland, OH 44106   | ship is seaworthy."
(216) 754-1691        |             -C.S. Lewis on Morality


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing