MEMSnet Home: MEMS-Talk: Mumps questions
Mumps questions
1999-09-22
Dung-An Wang
Mumps questions
Dung-An Wang
1999-09-22
--------------B14B4DD44ED358E4F35A6366
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

Hi MEMS friends
If I have a structure manufactured by MCNC MUMPs, a rectangle which
length
is L, width is W, height is H,  could I have the standard deviation and
average
of the L, W and H?  Or is there any other way (simulation software) to
estimate it?

Thank you for helping me out with that?


--
   Sincerely,
          Dung-An Wang

  Department of Mechanical Engineering    Ann Arbor, MI 48105
  3007 EECS, 2350 Hayward                 U.S.A.
  Ann Arbor, MI 48109-2125
  U.S.A.
E-Mail:
   [email protected]
Homepage:
   http://www-personal.engin.umich.edu/~wangd



--------------B14B4DD44ED358E4F35A6366
Content-Type: text/html; charset=us-ascii
Content-Transfer-Encoding: 7bit


Hi MEMS friends

If I have a structure manufactured by MCNC MUMPs, a rectangle which length
is L, width is W, height is H,  could I have the standard deviation and average
of the L, W and H?  Or is there any other way (simulation software) to estimate it?

Thank you for helping me out with that?
 

-- 
   Sincerely,
          Dung-An Wang


  Department of Mechanical Engineering    Ann Arbor, MI
48105
  3007 EECS, 2350 Hayward        &n
bsp;        U.S.A.
  Ann Arbor, MI 48109-2125
  U.S.A.
E-Mail:
   [email protected]
Homepage:
   http://www-
personal.engin.umich.edu/~wangd
  --------------B14B4DD44ED358E4F35A6366--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics