MEMSnet Home: MEMS-Talk: Selective release etch of Al sacrificial layer
Selective release etch of Al sacrificial layer
1999-01-12
Geng Chen
Selective release etch of Al sacrificial layer
Geng Chen
1999-01-12
Hi there,

We would like to release an Al sacrificial layer (0.5 µm thickness) without
affecting any
other metal and dielectric layers in the structure.  An undercut rate of 100
µm+ in 10
min. is required.  The etchant should not attack PE oxide, nitride, Ti, Au.
Any suggestions?
Your help will be very much appreciated.
Regards,

G. Chen


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics
University Wafer