MEMSnet Home: MEMS-Talk: Re: photomasks
Re: photomasks
1998-12-14
Allen Cowen
1998-12-14
Christopher Bang
1998-12-14
James Bustillo
1998-12-16
James van de Vyver
1998-12-17
Ken Westra
Re: photomasks
Ken Westra
1998-12-17
Kevin,

  We get our masks made by Adtek. They charge $ 250 US ($ 380 CND) for a
5" mask. Their address and phone number are:
    Adteck Photomask
    4950 Fisher Street
    Montreal Quebec Canada
    H4T 1J6
    (514) 737 7030
     514 737 9893 (fax)
     [email protected]

  Ken Westra
  MicroFab at the University of Alberta


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation