MEMSnet Home: MEMS-Talk: Re: Selective Ni etch
Re: Selective Ni etch
1999-01-25
Lawrence C. Gunn
Re: Selective Ni etch
Lawrence C. Gunn
1999-01-25
FeCl solution

On Thu, 14 Jan 1999, Noel A. Heiks wrote:

> Hello All:
> Can anyone receommend wet (or plasma) nickel etches that will not damage
> AlGaAs / GaAs?
>
> Thanks,
> Noel Heiks
> [email protected]
>
>
>


reply