Franck CHOLLET
SU-8 data
Franck CHOLLET
1999-02-10
Dear MEMS companions,
the thick photoresist SU-8 is becoming more and more important to the MEMS
community. However its use is far from easy, and standard photolythographic
process have to be substantially adapted.
To help beginners and others, a database on the subject, mixing literature
reference and experimental ones seems a good idea (a SU-8 FAQ in fact, that
surely rejoins the recent appeal for more information *exchange* in the
community :-). But it needs your help.
Those over there who possess data on the resist (ANY data: process data,
physical properties, characterisation results...), please send them to me,
and they will be included on a webpage with credits, of course.
Moreover, if you have already made a webpage on the subject, give me its
address and I will link it from the page.
The data already collected may be found at:
http://aveclafaux.freeservers.com/SU-8.html#top
As you may see it is just a beginning, but it will grow with your help!

Thank you,
Franck


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing