MEMSnet Home: MEMS-Talk: RE: Thick Resists for Au plating
RE: Thick Resists for Au plating
1999-02-10
Ramadas, Padmaja
1999-02-10
Sanjay Dhar
1999-02-15
Ramadas, Padmaja
1999-02-10
Ramadas, Padmaja
1999-02-10
Sanjay Dhar
1999-02-15
Ramadas, Padmaja
1999-02-15
Shekhar Bhansali
1999-02-19
Yohannes
RE: Thick Resists for Au plating
Sanjay Dhar
1999-02-10
AZ 4620 would be a good option. It is used for Au and Cu plating.

> ----------
> From:         Todd Green[SMTP:[email protected]]
> Reply To:     Todd Green;[email protected]
> Sent:         Tuesday, February 09, 1999 10:35 AM
> To:   [email protected]
> Subject:      Thick Resists for Au plating
>
> Hi,
>
> I'm looking for resists that can be spun up to around 25 microns and have
> good compatability with alkaline (pH=10) gold sulfite plating bath. We are
> using SJR 3740 but are interested in other alternatives. We tried SU-8
> but can't find anything to remove it. Is there anything else available?
>
> Thanks,
>
> Todd Green
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics