MEMSnet Home: MEMS-Talk: Re: TaAl etchant
Re: TaAl etchant
1998-11-29
SEED
Re: TaAl etchant
SEED
1998-11-29
Dear Shim,
    I suggest you trying to mix HF with H2SO4. The former is used to etch Ta
while the later etch Al. The mixing proportion depends on the contents &
structures of Ta and Al.

                                                                  Chao-Chen
Cheng