MEMSnet Home: MEMS-Talk: How does everybody cut the glass? (7740)
How does everybody cut the glass? (7740)
1999-03-17
Lee Jia-Hong
How does everybody cut the glass? (7740)
Lee Jia-Hong
1999-03-17
Hi, everybody:
    I am micromachining on 7740 glass, but I have problem to cut my 7740
glass into pieces, in order not to waste when experiments...
    Does anybody have good comments for me? or some experience to share...
thanks!
Best regards,
____________________________________________
Jerry Lee
(Jia-Hong Lee)
Insitute of Applied Mechanics,
National Taiwan University
Taipei, Taiwan, ROC
e-mail:
[email protected]
[email protected]
"Try then error is better than no try"


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group