MEMSnet Home: MEMS-Talk: Re: Etching Teflon
Re: Etching Teflon
1999-03-11
Fred Tepper
1999-03-11
Alexander Shenderov
1999-03-11
Jonathan Bernstein
1999-03-11
Fred Tepper
1999-03-11
Yohannes
1999-03-23
[email protected]
Re: Etching Teflon
Alexander Shenderov
1999-03-11
They do etch it with something like sodium naphtalate, but the
conditions are apparently somebody's trade secret (I am not even sure
whose).

Alex


reply