SU-8 photoresist
1999-01-28
Padmaja Ramadas
SU-8 photoresist
Padmaja Ramadas
1999-01-28
SU-8 is virtually insoluble in most chemicals if well crosslinked. You
would have to use RIE to etch off the SU-8.