David DeRoo
RE: Polysilicon - piezoresistive coefficients
David DeRoo
1999-03-15
A complete analysis of polysilicon piezoresitive coefficients is given in
David W. Burns Ph.D. thesis from the University of Wisconsin, 1988.

Regards,
David DeRoo
MicroSensors,Inc.

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Wednesday, March 10, 1999 8:50 AM
To: [email protected]
Subject: Polysilicon - piezoresistive coefficients


I'm looking for the transverse and the longitudinal piezoresistive
coefficients in the case using polysilicon thin film .... Thanks ...




_________________________________________________________
DO YOU YAHOO!?
Get your free @yahoo.com address at http://mail.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.