Re: How does everybody cut the glass? (7740)
Lee Jia-Hong
1999-03-24
Hi, Wen H. Ko:
    But thin glass as 500mu m is very fragile, can it be well cut with
diamond saw?
____________________________________________
Jerry Lee
(Jia-Hong Lee)
Insitute of Applied Mechanics,
National Taiwan University
Taipei, Taiwan, ROC
e-mail:
[email protected]
[email protected]
"Try then error is better than no try"


>Cut it with diamond saw as with Si or scrape lines with diamond tips then
>break.
>wen ko
>
>At 11:05 AM 3/17/99 +0800, you wrote:
>>Hi, everybody:
>>    I am micromachining on 7740 glass, but I have problem to cut my 7740
>>glass into pieces, in order not to waste when experiments...
>>    Does anybody have good comments for me? or some experience to share...
>>thanks!
>>Best regards,
>>____________________________________________
>>Jerry Lee
>>(Jia-Hong Lee)
>>Insitute of Applied Mechanics,
>>National Taiwan University
>>Taipei, Taiwan, ROC
>>e-mail:
>>[email protected]
>>[email protected]
>>"Try then error is better than no try"
>>
>>
>>
>>
>Wen H. Ko
>Phone: 1-216-368-2071
>FAX: 1-216-368-5326
>e mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics