Xiaoning Jiang
List of PZT thin disc suppliers
Xiaoning Jiang
1999-02-02
Hi, folks,

Thank you all for your replies to the above subject. As the requests from
other colleagues, I would like to post the replies here for your reference.

1. American Piezo Ceramics, Inc.
Duck Run, P.O. Box 1800, Mackeyville, PA 17750 USA
Phone 717-726-6961
fax 717-726-7466

2. Morgan Matroc
Electro Ceramics Division
232 Forbes Road
Bedford, Ohio, USA 44146
Tel: 440-232-8600, Fax: 440-232-8731

3. TRS Ceramics, Inc.
2820 E. College Avenue, Suite J
State College, PA 16801 USA
phone: 814/238-7485
fax: 814/238-7539
general e-mail: [email protected]

4. ValpeyFisher
   75 South Street, Hopkinton, MA 01748
   Phone: 508-435-6831
   Fax: 508-435-5289
   [email protected]


Small quantity order for research purposes can be made to the above
suppliers, but the minimum order may be over $500, the cutting charges are
exclusive. So, the small pieces of PZT thin disc (<5mm) are still a
concern, we tried the laser cutting recently and got initial success.

The replies from Prof. Rob Keynton, Mike Mladejovsky, Dr. Tianhong Cui, Dr.
Aiqun Liu are specially appreciated.

Thanks!

Best wishes,

Xiaoning


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation