MEMSnet Home: MEMS-Talk: Re: Does TMAH react with Teflon?
Re: Does TMAH react with Teflon?
1998-11-27
Alexander Hoelke
Re: Does TMAH react with Teflon?
Alexander Hoelke
1998-11-27
Certainly not. We have used it for quite some time.
--
Alexander Hoelke

graduate student

University of Cincinnati
ECE - CMSM

Phone:  (513)556-1997 / (513)556-4795
FAX:            (513)556-7326