Hi,

I remenber that there is a paper about the simulation in actuator and
sensor. You can check it

-----Original Message-----
From: Kavita Chandra [mailto:[email protected]]
Sent: Thursday, April 15, 1999 1:44 AM
To: [email protected]
Subject: Simulation of KOH etch



Does anybody has any information on a
software that simulates KOH/EDP etch of
silicon..(basically to get information
on issues like corner compensation,
under-cut).

Thanks,

Kavita Chandra


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Mentor Graphics Corporation