Hi everyone,

I have adhesion problems with AZ 4562 on gold at electroplating.
All kinds of pre-bake processes are not usefull.
Does anyone know a good adhesion promoter for gold like HMDS on SiO2 ?

Thank anyone very much in advance,

Sascha Kammer