MEMSnet Home: MEMS-Talk: RE: Anodic Bonding
RE: Anodic Bonding
2000-03-28
Lapp, Daniel S
2000-03-29
Mirza Andy
2000-03-31
Heeren, Henne van
RE: Anodic Bonding
Heeren, Henne van
2000-03-31
see: www.aml.co.uk, Experts on anodic bonding!!

regards

Henne van Heeren
OnStream B.V.
Lodewijkstraat 1
5652 AC Eindhoven
The Netherlands

tel  31 40 295 9815
fax 31 40 295 9906
email: [email protected]

The foundry for Micro System Technology


-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Friday, March 17, 2000 2:38 PM
To: [email protected]
Subject: Anodic Bonding


Hello,
I am working in silicon anodic bonding and I would like to have information
about this technique. I need the name of companies dealing this field,
since I want to buy the tools to implement it.
Thanks in advance,
Sandra

*********************************************************
Sandra Bermejo Broto
Semiconductor Devices Group (GDS)
Electronic Engineering Department
UPC-Campus Nord, C5
Jordi Girona, 1-3
E-08034 Barcelona
SPAIN
Phone: + 34 93 401 74 81
Fax:       + 34 93 401 67 56
e-mail: [email protected]
*********************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Addison Engineering
Process Variations in Microsystems Manufacturing