MEMSnet Home: MEMS-Talk: Re: Looking for glass (7740) substrate supplier
Re: Looking for glass (7740) substrate supplier
1996-04-03
[email protected]
1996-04-03
James P. Brody
1996-04-03
Robert Wood
1996-04-03
Justin D. Mansell
1996-04-03
Michael E. Poplawski
Re: Looking for glass (7740) substrate supplier
James P. Brody
1996-04-03
> I am looking for a supplier of
>         Corning 7740 (or equiv) substrates
>                 thickness 8 mils (+/-)
>                 diameter 2-4"
> to be used for bonding silicon wafers.
>
We use:

ESCO Products, Inc.
171 Oak Ridge Road
Oak Ridge, NJ 07438
Phone: (800) 922-3726

Last time I checked the thinnest stock they had (in 3" and 4" diameters) was 1
mm, but they'll do custom orders. It takes like 4-6 weeks.
--
Jim Brody     [email protected]
University of Washington  Center for Bioengineering


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation