MEMSnet Home: MEMS-Talk: Re: Indium plating on Gold
Re: Indium plating on Gold
2000-05-15
Prof. P Thareja
Re: Indium plating on Gold
Prof. P Thareja
2000-05-15
Subject:   electroplating Rhodium on gold pads

Sir,
We have not tried on Indium, but working on Rhodium and copper. Have you
done this kind of work? If yes , may we ask you for process parameters,
chemicals used, results obtained and  problems encountered ?

[email protected]
http://pthareja.bizland.com/
http://chandigarhfoundry.bizland.com/
Prof P Thareja
 # 662, Prof House,
 Punjab Engineering College,
 Chandigarh,160 012, INDIA
Tel 744101, Fax 91172746838
Fax on demand (Faxvoicemode) 745313 ( R)


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing