MEMSnet Home: MEMS-Talk: optical properties of silicon
optical properties of silicon
2000-05-15
YANG Jian-Yi
optical properties of silicon
YANG Jian-Yi
2000-05-15
Hi,

I'm looking for the refractive index and absorption coefficients of
silicon in the range from 1.2 to 1.6 um. Anyone know where I can find
them?

Thanks.

Jian-Yi
--
****************************************************
YANG Jian-Yi                            HAPPY or SAD
Dept of Information Science & Electronic Engineering
College   of   Information  Science  and  Technology
Zhejiang University,   Hangzhou 310027,    P.R.China
Tel:      +86-571-7951706(O)      +86-571-7979109(H)
Email:  [email protected]   [email protected]
****************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation
The Branford Group