Foturan cerematization
2000-06-14
Pramod Kolar
Foturan cerematization
Pramod Kolar
2000-06-14
Hi,

I would like to know how critical the cooling ramp is (the last step in
cerematization). I have a furnace which doesnt have active cooling. So, it
takes a while to cool off. Is it OK or can it lead to warping?

I had pretty severe warping in my sample. I welcome any suggestions as to
how I can overcome this  problem.

Thanks.

Regards,
Pramod Kolar

90291,                                          Ph: 919-660-5118 (Off)
Duke University,                                    919-383-2587 (Res)
Durham,NC 27708                                     919-660-5293 (Fax)


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review