At 14:48 -0400 6/26/2000, Luke Currano wrote:
>Can anyone tell me where I can get very thin bulk pzt (<125 microns) or
>bulk bending elements (<250 microns)?
>
>Thanks,
>Luke Currano
>University of Maryland MEMS Lab

Try American Piezo Ceramics.  I think they are in the Thomas Register.
They may only go to 10 mil (250 mu-m).  If you need to polish to get your
desired thickness, I would say look somewhere else for raw materials (there
must be other makers out there).  Polishing bulk wafers will frequently
depole them.

DD

--
David Drinkwater
3530 Bloomington Ave. S. #3
Minneapolis, MN 55407
Phone: 612.724.6359
[email protected]
http://www.demodave.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.