A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SAM solution.
SAM solution.
2000-09-07
Moonkyun Maeng
SAM solution.
Moonkyun Maeng
2000-09-07
Hi there,

I am a student in Georgia Tech.
I am fabricating some MEMS structure. Is there anybody
who knows how to make SAM(Self-Assembled Monolayer) solution, or
have done this SAM coating process actually.

If you have any information related to SAM (i.e commercial SAM solution
..), then let me know.

Thank you

Moonkyun Maeng
Georgia Institute of Technology, Atlanta Georgia, 30332
Email: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group