How to transfer 1 um pattern to Cr/Au
2000-10-03
Yahong Yao
How to transfer 1 um pattern to Cr/Au
Yahong Yao
2000-10-03
Hi, Folks,

I need make a multilayer structure. The layers are SiO2 (1.5 micron thick),
on top of that is Cr/Au ( 0.15 micron thick). Both layers have the same
pattern which is 1 micron structure with 1 micron space. How to transfer the
pattern? The key thing is how to pattern the metals with this fine features?

Thank you in advance.
Yahong
_________________________________________________________________________
Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com.

Share information about yourself, create your own public profile at
http://profiles.msn.com.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics