Re: Finding an etchant
2001-03-05
Roger Shile
Re: Finding an etchant
Roger Shile
2001-03-05
Aluminum etch (Phosphoric - Acetic acid based) is great for patterning Ni.
You can use Piranha to bulk strip the Ni.

>>> "Elizabeth Chalmers"  02/27/01 03:07PM >>>
Hi, I am an engineering student at Boston University
and I'm interested in finding an etchant (wet or
reactive ion gas) that will attack a nickel film
selectively, but leave the photoresist relatively
unetched.  Do you have any ideas?  Thank you very much
for your time,

Elizabeth Chalmers


__________________________________________________
Do You Yahoo!?
Get email at your own domain with Yahoo! Mail.
http://personal.mail.yahoo.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group