MEMSnet Home: MEMS-Talk: Low temperature micromachining with a-Si and polyimide
Low temperature micromachining with a-Si and polyimide
2001-03-23
Andrew Lee
Low temperature micromachining with a-Si and polyimide
Andrew Lee
2001-03-23
Hi everyone,

I am fabricating a device with doped a-Si film and polyimide as the
structural and sacrificial layer, respectively, on Si substrate with
integrated circuit. I have several questions about the fabrication.

1. How to realize the low temperature crystallization (<350^oC) of a-Si to
poly-Si.

2. It seems that polyimide sacrificial layer cannot be removed completely by
oxygen plasma ashing. How to remove the polyimide residue? The conventional
HF or H2SO4 based solution is not a good choice since it will attack metal
or dielectric insulating layer. An organic solution or a optimum dry etching
technique seems to be better. But I have no idea about it.

Any suggestion is appreciated.

Yours,
Andrew
_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation