MEMSnet Home: MEMS-Talk: blackening of St 101 getters
blackening of St 101 getters
2001-05-18
venkateshwaran pillai
blackening of St 101 getters
venkateshwaran pillai
2001-05-18
We are using zirconium non evaporable getters st 101 in our metal halide lamps.
sometimes after 15 minutes of burning or so, the getter turns blackinsh. Is it
due to formation of zirconium hydride. Even the base plate turns grayish.

Advanced thanks for any information.

Venkateshwaran. R



_____________________________________________________
Chat with your friends as soon as they come online. Get Rediff Bol at
http://bol.rediff.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.