MEMSnet Home: MEMS-Talk: Does anyone know of a source to have glass drilled?
Does anyone know of a source to have glass drilled?
2001-05-30
John Conklin
Does anyone know of a source to have glass drilled?
John Conklin
2001-05-30
Hello All,

    I need to have 4 mm diameter holes drilled into 4
mm thick soda lime glass.  The holes must have smooth
verticle sidewalls.  Thanks

John Conklin