MEMSnet Home: MEMS-Talk: need etchant for TiO2
need etchant for TiO2
2001-06-01
nakanishi tetsuya
need etchant for TiO2
nakanishi tetsuya
2001-06-01
Hi, I am an engineering student at Waseda University
in Japan.
I am looking for etchants(wet) for titanium dioxide.
Could anyone suggest a reference where these information would be
available. I have already tried HF, H2SO4 and NaOH.

Do you have any ideas?  Thank you very much for your time,

Tetsuya Nakanishi