Spherical shapes in Si
2001-08-16
Imad Yousef
Spherical shapes in Si
Imad Yousef
2001-08-16
Dear colleagues,

I am trying to etch silicon in spherical shapes. KOH
etching tends to create a flat bottom based on the
mask opening. Do you know of any other technique?

Regards,
Imad Yousef

__________________________________________________
Do You Yahoo!?
Make international calls for as low as $.04/minute with Yahoo! Messenger
http://phonecard.yahoo.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Mentor Graphics Corporation