MEMSnet Home: MEMS-Talk: BCB properties
BCB properties
2001-08-27
Randall Cha
2001-08-28
Alireza Modafe
BCB properties
Alireza Modafe
2001-08-28
Check out the following web site from Dow Chemical:
http://www.cyclotene.com

Good luck,
--Alireza Modafe

On Tue, 28 Aug 2001, Randall Cha wrote:

>
> Dear colleagues,
>
> I will like to ask if there is any source (website, literature, book)
> where I can know more about BCB (benzyocyclobutene). I will like to
> further explore its potential usuage in my MEMS works. I appreciate if
> anyone can send me some related info.
>
> Many thanks in advance,
> Randall
> DL, Singapore
>
> _______________________________________________
> mems-talk mailing list
> [email protected]
> To unsubscribe or change your list options, use:
>  http://fab.mems-exchange.org/mailman/listinfo/mems-talk
>

*******************************************************
*       Alireza Modafe                                *
*       Graduate Research Assistant                   *
*       MEMS Sensors and Actuators Lab (MSAL)         *
*       Dept. Electrical & Computer Engineering       *
*       University of Maryland                        *
*       College Park, MD 20742                        *
*       Phone: 301-405-1897                           *
*       Fax:   301-314-9281                           *
*       Email: [email protected]                    *
*       http://www.ece.umd.edu/~modafe                *
*******************************************************



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.