MEMSnet Home: MEMS-Talk: Hot Embossing Mould Insert
Hot Embossing Mould Insert
2001-08-31
Emer O'Reilly
2001-09-10
Luesebrink Helge
Hot Embossing Mould Insert
Luesebrink Helge
2001-09-10
Emer,

The most frequently used techniques are


CNC (Computerized Numerical Control):
Large Features, Stainless Steel, Robust
DEEMO (Dry-Etch Electroplate Mold):
Medium Features, Nickel, Robust
LIGA (LIthography, Galvanoformung, Abformung):
Small Features, Nickel, Short Life
Silicon Etch (Dry Etch, Wet Chemical Etch):
Medium Features, Silicon, Short Life

Best regards,
Helge






                -----Original Message-----
                From:   Emer O'Reilly [mailto:[email protected]]
                Sent:   Friday, August 31, 2001 6:52 AM
                To:     '[email protected]'
                Subject:        [mems-talk] Hot Embossing Mould Insert

                Hi all.

                I am researching different possibilities to make a mould
insert for our hot
                embosser. Apart from the LIGA technique and etching of
silicon, has anyone
                any experience of other ways and materials?

                Thanks

                Emer



                _______________________________________________
                mems-talk mailing list
                [email protected]
                To unsubscribe or change your list options, use:
                 http://fab.mems-exchange.org/mailman/listinfo/mems-talk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review