MEMSnet Home: MEMS-Talk: Info regarding Invar plating
Info regarding Invar plating
2001-09-16
madhulika sathe
Info regarding Invar plating
madhulika sathe
2001-09-16
I am currently involved in plating Ni-Fe alloy.I would like to find out the
essentials required for the process.I am facing problems when plating it on
nickel sidewalls.

Thanks,

Madhulika Sathe
Research Assisstant
Mechanical Engineering Dept.
Louisiana State University
Baton Rouge , LA - 70803

Phone : (225)578-4412
Fax   : (225)578-9195





Join 18 million Eudora users by signing up for a free Eudora Web-Mail account at
http://www.eudoramail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing